What to close the cracks in the log

What to close the cracks in the log

With all the advantages of wood, natural disadvantages are characterized - drying, shrinkage and tapping, so defects arise on the log on the log. Most of them can be eliminated by their own hands.

1
Transverse splits appear due to loading or overload, such details are not repaired, but only replaced. Small longitudinal cracks are eliminated by special sealantFor wider (from 5 mm) there is a technology that includes insulation and hermetic sealing of seams.

2
For repair, you will need:

  • The filler is the thermal insulation harness "EnergoFlex" (replaced by packles, felt or just foam);
  • Sealant - Neomid or Evrotex;
  • Knife, scraper;
  • Rubber spatula;
  • Manual sprinkler for water.

Pre-internal cavities are processed by the antiseptic composition, then the walls are dried. All further work is made on dry brings.

3
The order of sealing cracks in the log:

  1. Splits are cleaned with chips, sawdust and loose wood.
  2. Filler is laid in crack - about half of its depth;
  3. Next, the remaining cavity is filled with sealant;
  4. With the help of a spatula, the edges are smoothed so that a smooth surface has come out - it is easier to do if splashing on a sealant from the sprayer;
  5. The surplus is removed with a rap and the time is withstanding to completely dry the seam.

4
The slots between the logs are sealed by dry filling - caulking. A package is used as a placeholder, felt or jute. First, the material is shred into the joint with a wooden blade, then tapping in it with a color, is finally compacted until it becomes spring. The protruding residues are cut off with a knife or a grinder with a mounted petal circle.

5
It is convenient to use ready-made sealing compositions, but they all possess one disadvantage: after a few years, wood will dry and crack will appear again. This minus is deprived of a permanent moss, which is soaked with water before use 30 minutes, and during drying it increases by 20%, thereby thoroughly blocking the gaps.